Nylon is one of the most widely used and versatile thermoplastic resins. Its combination of physical properties versus its price makes it a favorite choice for numerous applications. Nylon has a consistent history of replacing other materials including: metal, brass, bronze, aluminum, and rubber. In replacing metal gears in machinery, nylon can be advantageous because of its ability to reduce noise, use less lubrication and increase gear life. TECAMID™MDS is an extruded "moly" filled nylon 6/6, which is gray in color. The addition of particles of molybdenum disulfide enhances the surface lubricity and wear resistance over unfilled nylon. In applications requiring high lubricity, this material may be a good candidate. In addition to the greater lubricity there are many additional property enhancementsthat occur.
- Low surface friction
- Increased surface hardness
- Increased heat resistance
- Higher tensile properties
- Improved dimensional stability
TECAMID™MDS has enhanced properties which make it an ideal material to replace metals in machinery. It can increase the life of many moving parts as well as provide a noise reduction benefit and requires less lubrication. A very stable compound with many industrial applications. | | Properties | ASTM Test Method | Units | Tecamid™MDS |
|---|
| Physical | Density | D792 | lbs/in3 | 0.0412 |
|---|
Specific Gravity | D792 | g/cc | 1.14 | Water Absorption, @24 hours, 73°F | D570 | % | 1.2 - 2.5 | @Saturation, 73°F | D570 | % | 7.5 - 8.5 | | Mechanical | Tensile Strength @ Yield, 73°F | D638 | psi | 11,000 |
|---|
Tensile Modulus | D639 | psi | 450,000 | Elongation @ Break, 73°F | D638 | % | 15 | Flexural Strength, 73°F | D790 | psi | 17,000 | Flexural Modulus, 73°F | D790 | psi | 450,000 | Compressive Strength | D695 | psi | - | Izod Impact Strength, 73°F | D256 | ft-lbs/in | 1.2 | Rockwell Hardness, 73°F | D785 | M Scale | M 87 | Shore Hardness | - | D Scale | - | Wear Factor Against Steel, 40 psi, 50 fpm | D3702 | in3 1
--- x ---
hr PV | 1.9 x 10-8 | Static Coefficient of Friction | D3702 | - | | Dynamic Coefficient of Friction, 40 psi, 50 fpm | D3702 | - | | | Thermal | Heat Deflection Temperature @ 66 psi | D648 | °F | 470 |
|---|
@264 psi | D648 | °F | 194 | Coefficient of Linear Thermal Expansion | D696 | in/in/°F | 4.0 x 10-5 | Maximum Servicing Temperature, Intermittent | - | °F | 355 | Long Term | UL746B | °F | 230 | Specific Heat | - | BTU/lb-°F | 0.4 | Thermal Conductivity | - | - | 1.7 | Melting Point | D3418 | °F | 491 | Flammability | UL94 | (mm) | HB | | Electrical | Surface Resistivity | D257 | ohm/square | - |
|---|
Volume Resistivity | D257 | ohm-cm | 1015 | Dielectric Strength | D149 | V/mil | 30 | Dielectric Constant, @ 60 Hz, 73°F, 50% RH | D150 | - | 2.5 | @ 1 MHz | D150 | - | | @ 20 GHz | D150 | - | | @ 30 GHz | D150 | - | | Dissipation Factor, @ 60 HZ, 73°F | D150 | - | | This information is only to assist and advise you on current technical knowledge and is given without obligation or liability.
All trade and patent rights should be observed. All rights reserved. Data obtained from extruded shapes material.
TECAMID™MDS = Ensinger Industries, Inc. |
|